Time Temperature Transformation Diagrams

Time Temperature Transformation Diagrams Time has influence on phase transformation. The rate of transformation is dependent on the time and the temperature. Phase diagrams describe equilibrium microstructural development which is achieved at extremely slow cooling or heating conditions. The phase diagrams give no information on the time which is taken to form a phase as …

Read More

Phase Diagrams

Phase Diagrams A phase in a material is a region which differ in its microstructure and or composition from another region. It is homogeneous in crystal structure and atomic arrangement and has same chemical and physical properties throughout. It has a definite interface and able to be mechanically separated from its surroundings. A component is …