Glossary of technical terms for the use of metallurgical engineers   Terms starting with alphabet ‘B’

Glossary of technical terms for the use of metallurgical engineers Terms starting with alphabet ‘B’ Babbitt metal, Babbitt – It is a non-ferrous bearing alloy originated by Isaac Babbitt in 1839. Presently, the term includes several tin-base alloys consisting mainly of different quantities of copper, antimony, tin, and lead. Lead-base Babbitt metals are also used. …