Rolling of steel and major equipment in a Cross-country Rolling Mill

Rolling of steel and major equipment in a Cross-country Rolling Mill Most of the steel products are rolled from the cast products from continuous casting machine through a series of rolling and finishing operations. The process is called simple rolling, when two rolls of equal diameter and with axis lying in same plane rotate in …