Tag

Rolling of Steel Plates in a Plate Rolling Mill

Rolling of Steel Plates in a Plate Rolling Mill Plate steel is defined as a flat, as-rolled or heat treated product of thickness of at least 5 mm and width of at least 1,200 mm. Plate steel is widely used steel product. It falls normally in the categories of carbon steel, high strength low alloy …