Fusion Bonded Epoxy Coating of Steel

Fusion Bonded Epoxy Coating of Steel Fusion bonded epoxy (FBE) coating of steel materials is primer less, one-part, heat curable, thermosetting powdered epoxy coating which is designed to provide maximum corrosion protection to the substrate steel. It is a coating of very fast curing, thermosetting protective powder which utilizes heat to melt and adhere the …