Comparison of By-product Coke Ovens and Heat Recovery Coke Ovens
…structure. Hence, the heat-recovery oven coke demonstrates better carbon structural development. For the by-product oven coke, carbon structural development seems to have a stronger impact on CSR than surface area…
Read More