Lubricants satyendra May 20, 2013 1 Comment Demulsibility, Flash point, Friction, grease, Lube, lubricants, lubrication, Mineral oils, pour point, Stribeck curve, Synthetic fluids, Vegetable oils, viscosity, Read More
Glossary of Terms used in Galvanizing of Steel satyendra May 15, 2013 26 Comments Delta laye, Dross, Dry galvanizing, Eta layer, galvanizing. corrosion, gamma layer, glossary, Hot dip process, Wet galvanizing, Zeta layer, Read More
Advanced High Strength Steels for Automotive Application satyendra May 12, 2013 0 Comments AHSS, BH steel, CP steel, DP steel, FB steel, HF steel, HSLA steel, HSS, IF steel, MS steel, PFHT steel, TRIP steel, TWIP steel, Read More
Reinforcement Steel satyendra May 10, 2013 4 Comments corrosion resistance, CTD bars, Ductility, Micro alloying, Rebars, reinforced concrete, reinforcement steel, TMT rebars, Yield strength, Read More
Limestone and Dolomite and their Use in Iron and Steel Plant satyendra May 8, 2013 5 Comments basic, Calcined dolomite, dolomite, flux, lime, limestone, neutraliziing, Sintered dolomite, slag, Read More
Rails and Rail Steel satyendra May 5, 2013 14 Comments Axle load, bainite, Brittle failure, carbon manganese steel, Head hardening, pearlite, Rail profile, Rolling contact fatigue, Wear resistance, Read More
Spring Steels satyendra May 2, 2013 2 Comments Fatigue strength, helical spring, high carbon steel, leaf spring, Relaxation, spring steel, stainless steel, Tempered and hardened steel, Read More
Cold Heading Quality Steels and Cold Heading Process satyendra April 30, 2013 0 Comments CHQ, Cold forging, cold heading, Cold heading equipment, fastener, upsettability, Read More
Weathering Steels satyendra April 27, 2013 2 Comments Adhering oxide layer, atmospheric corrosion, COR-TEN steel, Patina, Rust, weathering steel, Read More
Electrical Steels satyendra April 25, 2013 2 Comments CGO, CRGO, CRNGO, eltrical sheets, GOES, HGO, hyatersis, lamination, magnetic proerties, NOES, Read More