Important Features of Rolling of Wire Rods Mar27

Important Features of Rolling of Wire Rods...

Important Features of Rolling of Wire Rods Wire rods are normally rolled in a high speed rolling mill, where steel temperature is above 1,000 deg C, maximum speed of rolling exceeds 120 metres per second (m/s) and coils of wire rod produced can be upto 10 kilometers (km) long. During rolling of wire rods, usually 25 passes to 30 passes are taken in a continuous rolling mill. Wire rod is a material which has a very wide application. From components for the automotive industry, tire cord, electrodes, connecting elements such as nuts and bolts, springs, wire and wire products, steel reinforcements, and so on, everything is based on wire rod. That is why wire rod mill is normally designed with versatility in mind. The mill being an energy intensive mill, it becomes necessary that the optimum solutions are incorporated in the mill design without compromising on the flexibility. All size ranges, materials and alloys need to be produced efficiently and with high productivity in the wire rod mill. Wire rods are required to meet the wire rod users’ requirements of surface and internal quality as well as physical, chemical, mechanical, and metallurgical properties. Wire rods undergo post-processing such as drawing, forging, or machining into desired shapes and heat treatment for enabling the product to achieve the desired strength. Thus, the wire rods are required to be capable of ensuring good performance of the produced parts wherever they are used, and at the same time, to have good workability at different stages of the post-processing. The user of wire rods has three basic requirements namely (i) to eliminate or simplify one or more of the secondary or tertiary processing to improve productivity and reduce processing cost, (ii) to improve the functionality, i.e. to extend the...

Main Features of a Modern Bar and Light Section Mill Feb01

Main Features of a Modern Bar and Light Section Mill...

Main Features of a Modern Bar and Light Section Mill The objective of a bar and light section mill is to reheat and roll steel billets into bars and light sections. The production of bar and light sections in these mills is subject to constant change. There is growing demands on the quality of these products as well as on the flexibility and cost effectiveness of these mills. This has necessitated the development of new and innovative technologies and processes. Modern bar and light section mills are high speed mills capable of rolling bars and light sections of special bar quality grades and engineering steels at high production rates, while keeping investments and operating costs at the reasonable levels. Modern bar and light section mills are expected to meet the following requirements. High mill availability coupled with high productivity and high yields. Meeting the need of low maintenance. Meeting the need of lower energy consumption. Close dimensional tolerances. Negative tolerances (In sectional weight). No variation in dimensions throughout the length. Uniform physical properties. For achieving these demanding requirements, many important features are incorporated in the modern bar and light section mills. Some of these are described below. Reheating furnace – Modern bar and light section mills are equipped with energy efficient walking beam furnaces which are normally computerized controlled. These reheating furnaces uniformly heat the billets to the target temperatures at the required production rates and without skid marks and without cold spots. These furnaces are capable of receiving cold or hot billets as the charge material in the furnace. The modern reheating furnaces have the features of (i) superior heated billet quality, (ii) better heating efficiency, (iii) very low fuel consumption, (iv) minimum scale loss, contributing to achieving high material yield, (v) low...