Dolomite – Its Processing and Application in Iron and Steel Industry Dolomite is an anhydrous carbonate mineral. It is a double carbonate of calcium and magnesium (CaCO3.MgCO3). It is one of the important raw materials used in production of iron and steel. Dolomite contains theoretically 54.35 % of CaCO3 and 45.65 % of MgCO3 or 30.41 % of CaO, 21.86 % of MgO, and 47.73 % of CO2. However, in nature, dolomite is not available in this exact proportion. Hence generally the rock containing in the range of 40 % to 45 % of MgCO3 is usually called dolomite. The main uses of dolomite in iron and steel industry are (i) as a fluxing material (ii) for protection of refractory lining, and (iii) as a refractory raw material. Dolomite in iron and steel industry is normally used in three forms. These are (i) raw dolomite which is also the natural form of dolomite, (ii) calcined dolomite, and (iii) sintered dolomite. When dolomite is used as a fluxing material then it is used as either raw dolomite or calcined dolomite. When dolomite is used for the protection of refractories, it is used in calcined form and when dolomite is being used as a refractory raw material, it is used in the form of sintered dolomite. The uses and form of dolomite in iron and steel industry is shown in Fig 1. Fig 1 Uses and form of dolomite in iron and steel industry Processing of dolomite Dolomite after its mining has to undergo several processing before it can be used in various processes. The basic processes in the production of dolomite are (i) quarrying of raw dolomite, (ii) preparing mined dolomite for its use by crushing and sizing, (iii) calcining of raw dolomite, (iv) processing...