Oxygen Blowing Lance and its Role in Basic Oxygen Furnace In the basic oxygen furnace (BOF) steel making a water-cooled lance is used for injecting a high velocity (super-sonic) stream of oxygen onto the liquid bath for its refining. The velocity or momentum of the oxygen jet results in the penetration of the liquid slag and metal to promote oxidation reactions over a relatively small area. The velocity of the oxygen jet and the penetration characteristics are functions of the nozzle (lance tip) design. The top-blowing lance oxygen jet of the BOF converter works as the source of feeding oxygen and energy for stirring of the liquid metal in the bath. Major in-furnace phenomena of a BOF converter that involve the top-blowing lance oxygen jet are formation of a cavity as a result of physical interaction between the oxygen jet and liquid metal, stirring of liquid metal, generation of spitting and dust, and post combustion of CO gas generated by decarburization and reaction with oxygen. For the optimization of BOF converter operation and control the above phenomena, different devices and improvements have been made and applied to the design and operation of top-blowing lance. Examples of these include the employment of Laval nozzles capable of converting pressure energy to jet kinetic energy with high efficiency in order to promote stirring of liquid metal, and the use of a multi-hole lance that enables high-speed oxygen feeding while suppressing generation of spitting and dust by dispersing of the oxygen jet. With the introduction of combined blowing in the BOF converters, the role of top-blowing lance jets as the source of energy for stirring liquid metal iron declined and flexibility in design and operation has been enhanced significantly. The main reason for blowing oxygen into the liquid...