Ferro-Silicon

Ferro-Silicon Ferro-silicon (Fe-Si) is a metallic ferro-alloy having iron (Fe) and silicon (Si) as its main elements. In commercial terminology It is defined as a ferro-alloy containing 4 % or more of Fe, more than 8 % but not more than 96 % of Si, 3 % or less phosphorus (P), 30 % or less of manganese (Mn), less than 3 % of magnesium (Mg), and 10 % or less any other element. However, the regular grades of the ferro-alloy normally contain Si in the range of 15 % to 90 %. The usual Si contents in the Fe-Si available in the market are 15 %, 45 %, 65 %, 75 %, and 90 %. The remainder is Fe and minor elements. The minor elements, such as aluminum (Al), calcium (Ca), carbon (C), manganese (Mn), phosphorus (P), and sulphur (S) are present in small percentages in Fe-Si. Commercially, Fe-Si is differentiated by its grade and size. Fe-Si grades are defined by the percentages of Si and minor elements contained in the product. The principal characteristic is the percentage of Si contained in the ferro-alloy and the grades are referred to primarily by reference to that percentage. Hence 75 % Fe-Si contains around 75 % of Si in it. Fe-Si grades are further defined by the percentages of minor elements present in the product. ‘Regular grade 75 % Fe-Si’ denote that the product containing the indicated percentages of Si and recognized maximum percentages of minor elements. Other grades of Fe-Si differ from regular grades by having more restrictive limits on the content of elements such as Al, titanium (Ti), and/or Ca in the ferro-alloy. Fe-Si is also produced in a grade that contains controlled amounts of minor elements for the purpose of adding them to...