Coal for Pulverized Coal Injection in Blast Furnace...

Coal for Pulverized Coal Injection in Blast Furnace Injection of pulverized coal in the blast furnace (BF) was initially driven by high oil prices but now the use of pulverized coal injection (PCI) hasĀ  become a standard practice in the operation of a BF since it satisfy the requirement of reducing raw material costs, pollution and also satisfy the need to extend the life of ageing coke ovens. The injection of the pulverized coal into the BF results into (i) increase in the productivity of the BF, i.e. the amount of hot metal (HM) produced per day by the BF, (ii) reduce the consumption of the more expensive coking coals by replacing coke with cheaper soft coking or thermal coals, (iii) assist in maintaining furnace stability, (iv) improve the consistency of the quality of the HM and reduce its silicon (Si) content, and (v) reduce greenhouse gas emissions. In addition to these advantages, use of the PCI in the BF has proved to be a powerful tool in the hands of the furnace operator to adjust the thermal condition of the furnace much faster than what is possible by adjusting the burden charge from the top. Schematic diagram of a BF tuyere showing a pulverized coal injection lance is at Fig 1. Fig 1 Schematic diagram of a BF tuyere showing a pulverized coal injection lance Several types of coals are being used for PCI in the BF. In principle, all types of coals can be used for injection in BF, but coking coals are not used for injection since they are costly, have lower availability and are needed for the production of coke. Also, if coking coals are used for injections in BF, They lead to tuyere coking. Hence, coals used for injection...