Silica and its role in the production of iron and steel...

Silica and its role in the production of iron and steel Silicon, the element, is the second most abundant element in the earth’s crust. Silica is the scientific name for a group of minerals made of silicon and oxygen. It is one of the most abundant oxide materials in the earth’s crust and is found in most mineral deposits found on the earth. It is the starting material for the production of ceramics and silicate glasses. Silica (from the Latin word ‘silex’), is an oxide of silicon. It is a compound made up of silicon and oxygen atoms and has the chemical formula SiO2. It occurs commonly in nature as sandstone, silica sand or quartzite. It is the most frequently found in nature as quartz (SiO4). It is the major constituent of sand. Silica is one of the most complex and most abundant families of materials, existing as a compound in several minerals. Silica occurs in a variety of crystalline modifications and also as an under-cooled melt called quartz glass. The crystal structure of the individual SiO2 modifications can differ widely, so that distinct density changes occur during transformation. This is of great importance during heating and cooling because of the change in the volume. Silica can be a naturally occurring substance, like quartz, or it can result from human activities. It occurs in many forms. It can exist in an amorphous form (vitreous silica) or in a variety of crystalline forms. Amorphous silica is found in nature (e.g., diatomaceous earth and plants), as well as in synthetic materials. In amorphous silica, the silicon and oxygen atoms are not arranged in any particular pattern. Amorphous forms of silica have a random pattern while in crystalline silica, atoms of silicon and oxygen are arranged in a repeating, three dimensional pattern which is known as crystal lattice. Crystalline silica...

Induction Furnace Refractory Lining with Silica Ramming Mass...

Induction Furnace Refractory Lining with Silica Ramming Mass Induction furnaces are used for melting cast iron, mild steel and various alloy steels in foundries and making of steel in mini steel plants using sponge iron. Lining is the important part of induction furnace. Furnace performance is directly related to the performance of its lining. Well laid and stabilized lining results in smooth working of furnace, optimum output, and good control of the metallurgical reactions. The lining practice best suited to a particular furnace depends upon the capacity and design of the furnace, operation practice adopted during making of a heat, and furnace output. For successful and consistent performance of the lining, the important aspects are (i) use of proper grade and quality of the lining material, (ii) careful and systematic lining practice, and (iii) consistency in working conditions.  Fig 1 shows the installed refractory lining of a coreless induction furnace, Fig 1 Installed refractory lining of a coreless induction furnace The characteristics of the lining material needed for consistent lining life include (i) thermal characteristics which means that it has to withstand the stresses developed by thermal cycles during the furnace operation, (ii) chemically inert to metal being melted, (iii) structural strength under operating conditions, (iv) high erosion resistance, (v) ease of installation, (vi) reparability of the lining, (vii) ease of dismantling, and (viii) economics. As such, it is very difficult to judge the suitability of a particular lining under various conditions like operating temperature, metal being melted, the type of formed slag, and furnace capacity. Chemical inertness to the liquid metal can be achieved by using acid and neutral lining for the acidic slag and neutral or basic lining for the basic slags. Normally, the selection of refractory for the furnace lining is...

Refractories and Classification of Refractories...

Refractories and Classification of Refractories Refractories are inorganic, nonmetallic, porous and heterogeneous materials composed of thermally stable mineral aggregates, a binder phase and additives. The principal raw materials used in the production of refractories are normally the oxides of silicon, aluminum, magnesium, calcium and zirconium. There are some non-oxide refractories like carbides, nitrides, borides, silicates and graphite. Refractories are chosen according to the conditions they face during their use. Some applications require special refractory materials. Zirconia is used when the material is required to withstand extremely high temperatures. Silicon carbide and carbon are two other refractory materials used in some very severe temperature conditions, but they cannot be used in contact with oxygen, since they oxidize and burn in atmospheres containing oxygen. Refractories are the materials which are resistant to heat and exposure to different degrees of mechanical stress and strain, thermal stress and strain, corrosion/erosion from solids, liquids and gases, gas diffusion, and mechanical abrasion at various temperatures. In simplified language, they are considered to be materials of construction which are able to withstand high temperatures. Refractories are usually inorganic non-metallic materials with refractoriness greater than 1500 deg C. They belong to coarse-grained ceramics having microstructure which is composed of large grains. The basis of body is coarse-grained grog joined by fine materials. Refractory products are a specific sort of ceramics that differs from any ‘normal’ ceramics mainly with their coarse-grained structure being formed by larger grog particles joined by finer intermediate materials (bonding). ASTM C71 defines refractories as ‘non-metallic materials having those chemical and physical properties that make them applicable for structures or as components of systems that are exposed to environments above 538 deg C’. Refractories are to be chemically and physically stable at high temperatures. Depending on the operating environment, they...

Introduction to Refractories...

Introduction to Refractories Refractories are defined in ASTM C71 as non metallic materials having those chemical and physical properties that make them applicable for structures or as components of systems that are exposed to environments above 538 deg C. Refractories are inorganic, nonmetallic, porous and heterogeneous materials composed of thermally stable mineral aggregates, a binder phase and additives. These materials have ability to retain its physical shape and chemical identity when subjected to high temperatures. Refractories perform four basic functions namely (i) act as a thermal barrier between a hot medium and the wall of the containing vessel, (ii) represent a chemical protective barrier against corrosion, (iii) ensure a physical protection, preventing the erosion of walls by the circulating hot medium and (iv) act as thermal insulation for heat retention. Refractories are classified in the different following ways. Classification based on chemical composition –  Refractories are classified on the basis of their chemical behaviour into following three classes. Acid refractories – These are those refractories which are attacked by alkalis or basic slags. These are used in acidic atmosphere or where slags are acidic. Example of these refractories are silica and zirconia. Basic refractories – These refractories are attacked by acid slags but stable to alkaline slag, dust and fumes at the elevated temperatures. These refractories are used in alkaline atmospheres. Example of these refractories are magnesia, dolomite and chromite. Neutral refractories – These refractories are chemically stable to both acids and bases and used in the areas where slag and environment are either acidic or basic. Examples are carbon graphite, chromites and alumina. Grphite is the least reactive and is extensively used in the furnaces where the process of oxidation can be controlled. Classification based on physical form – Refractories are classified according...